Hot-Working Window Identified for Crack-Prone Al-20Sc Alloy
An experimental study found stable hot working of Al-20Sc alloy at 550–600 °C and 0.01–0.1 s⁻¹, with cracks concentrated in ...
An experimental study found stable hot working of Al-20Sc alloy at 550–600 °C and 0.01–0.1 s⁻¹, with cracks concentrated in ...