A systematic review published in Progress in Orthodontics reveals that clear aligners undergo clinically relevant degradation in physical, mechanical, and morphological properties during use, while their core chemical structures remain largely stable. The study, conducted by Nabeel Almotairy, Fahad Aleisa, and Abdulrahman K. Alshammari, synthesized evidence from ninety-five studies to evaluate how aging affects these orthodontic devices across different material types and commercial brands. The findings indicate that thermoplastic polyurethane-based aligners and directly printed aligners are generally more susceptible to deterioration than polyethylene terephthalate glycol-modified aligners, although results regarding specific properties like hardness and stiffness were inconsistent across the reviewed literature.
The research team registered their protocol in PROSPERO and followed the PRISMA 2020 guidelines to ensure a rigorous search and selection process. They searched five electronic databases, including PubMed, Web of Science, MEDLINE, ProQuest, and Scopus, for studies published up to March 18, 2026. The eligibility criteria focused on studies assessing clear aligner properties after intraoral use or simulated aging through methods such as thermocycling, cyclic loading, or liquid immersion. This comprehensive approach allowed the authors to compare aging characteristics across various polymer compositions, including polyurethane, polypropylene, and proprietary formulations, as well as photopolymer resins used in 3D printing.
Chemical stability emerged as a consistent theme in the review, with Fourier-transform infrared spectroscopy revealing no significant molecular degradation in most aligner materials during aging. However, the study noted that some brands exhibited trace elemental release, including mercury from Eon aligners and aluminum and silicon from Invisalign aligners after intraoral use. While the bulk molecular architecture of thermoplastic aligners appears resistant to hydrolytic or oxidative degradation, the release of these trace elements suggests that ongoing biocompatibility evaluation may be warranted, particularly given the cumulative exposure over a full orthodontic treatment course.
Physical properties, particularly discolouration and water sorption, showed significant changes following exposure to staining solutions and oral fluids. The review calculated a pooled weighted mean for discolouration after seven-day immersion in coffee, tea, or red wine at 37 degrees Celsius. Coffee produced the greatest colour change, with a weighted mean Delta E of 70.9, compared to 18.4 for tea and 11.5 for red wine. Invisalign aligners consistently exceeded the clinically perceptible threshold of Delta E 3.7 across all three staining solutions, indicating that aesthetic acceptability may be compromised even with compliant cleaning regimens, especially for strongly pigmented beverages.
This increased water uptake may induce physicochemical alterations that lead to mechanical deterioration and swelling. The review suggests that moisture penetration can disrupt polymer chain packing, increasing free volume and creating pathways for further water diffusion. Since each aligner is designed to deliver approximately 0.25 to 0.30 millimeters of tooth movement per wear cycle, any dimensional changes could effectively displace space intended for tooth movement, potentially reducing the efficiency of force delivery.
Mechanical degradation was a central focus of the review, with stress relaxation and force decay being particularly notable. The study found that force decay of 40 to 90 percent typically occurred within the first 48 hours of wear, depending on the force type and material. This rapid decline suggests that the effective therapeutic window of a single aligner tray may be considerably shorter than typical replacement intervals of one to two weeks. Although none of the included studies directly measured tooth movement outcomes, the authors hypothesize that meaningful orthodontic force delivery is concentrated in the early days of wear, a finding that warrants confirmation through studies correlating in vitro force decay with clinical tooth movement.
The review also highlighted material-specific differences in mechanical performance. Thermoplastic polyurethane-based aligners, such as Zendura, generally exhibited higher tensile strength and elastic modulus than polyethylene terephthalate glycol-modified aligners like Duran and Erkodur. However, directly printed aligners showed greater susceptibility to force decay and stiffness reduction compared to thermoformed alternatives. The authors noted that print parameters, such as layer thickness and build orientation, significantly influenced the colour stability and mechanical properties of directly printed aligners, with a 50-micrometer layer thickness and 90-degree build orientation producing the greatest colour stability.
Morphological changes, including surface roughness, cracks, and porosity, were also documented following aging. Intraoral use and simulated aging led to the formation of microcracks, surface voids, and delamination in various aligner materials. These structural changes may compromise force delivery and increase pigment penetration, while also raising concerns regarding bacterial biofilm accumulation and microplastic leaching. The review found that surface roughness increased in thermoplastic polyurethane-based aligners after thermocycling, while polyethylene terephthalate glycol-modified aligners showed more variable responses depending on the specific brand and aging protocol.
Risk of bias assessment revealed that the majority of included studies had moderate or high risk of bias, with common limitations including lack of blinding, inadequate randomization, and insufficient reporting of operator reliability. The authors acknowledged that the considerable methodological heterogeneity across studies, including differences in aging protocols, specimen preparation, and outcome measurement techniques, made direct comparisons challenging. This heterogeneity, combined with the inherent limitations of in vitro models in replicating the complex oral environment, suggests that the certainty of evidence for the reported aging effects is low to moderate.
The review concludes that while clear aligner materials maintain chemical stability, they undergo clinically relevant degradation in physical, mechanical, and morphological properties during use. Clinicians may need to prioritize material-specific protocols, reinforce dietary and cleaning instructions, and consider force decay when determining aligner replacement intervals. The findings underscore the need for standardized aging protocols, longitudinal clinical studies with patient-centered outcomes, and dedicated evaluation of emerging directly printed aligner materials to advance evidence-based practice in clear aligner therapy.
Beyond broad polymeric classifications, the specific commercial systems evaluated across the ninety-five papers revealed notable distinctions during experimental testing. Polyethylene terephthalate glycol-modified materials were investigated across numerous brands, including Duran, Erkodur, Essix A+, CA Clear Aligner, Clear Cap, CA-medium, K line, and Smartee. Polyurethane and thermoplastic polyurethane configurations included F22 Evoflex, Zendura, Spark, and Invisalign, alongside smaller subsets of polycarbonate and polypropylene products such as Angel aligner. Several investigations tested hybrid configurations, including multilayered poly(ester-urethane) or polycarbonate-urethane formulations, as well as photopolymer resins used in direct 3D printing such as Dental LT Clear and Tera Harz TC-85. The geographic origin of the underlying literature was notably broad, with twenty-three studies originating from Italy, and the vast majority appearing in print from 2020 onward.
Experimental conditions varied substantially in how researchers mimicked the oral cavity. Fifty investigations relied on static or dynamic immersion across a wide variety of fluids, including artificial saliva, distilled water, cola, fruit juice, red wine, coffee, tea, nicotine solutions, and dedicated aligner cleaning agents. Other laboratories introduced thermal fatigue via thermocycling, alternating between hot and cold temperature baths to approximate clinical ingestion cycles. Mechanical stress was similarly reproduced through static load deflections, stress relaxation protocols, or cyclic compression designed to simulate repeated chewing forces. In contrast to purely benchtop simulations, twenty-four studies evaluated aligners retrieved after direct intraoral wear, where patients had used the appliances continuously for typical clinical intervals of seven or fourteen days.
Detailed physical testing showed that thermal and optical behaviours diverge across resin formulations. Thermoplastic polyurethane aligners exhibited glass transition temperatures above 95 degrees Celsius, compared to 80 to 89 degrees Celsius for polyethylene terephthalate glycol-modified aligners. Directly printed resins recorded a significantly lower glass transition temperature of 69.45 degrees Celsius, reflecting earlier entry into a viscoelastic state and potentially lower thermal stability. Optical transparency was generally unaffected by immersion in neutral saliva or water, but decreased substantially following exposure to red wine, coffee, smoking, or alcohol. For directly printed aligners, surface transparency dropped markedly after immersion in turmeric, which produced stronger staining than coffee or tea. Cleaning regimens showed variable effectiveness, with denture cleansers and colourant-free soap causing minimal colour shifts, whereas whitening toothpastes and certain cleaning crystals caused noticeable alterations.
Mechanical evaluations of stiffness and deformation exposed further differences between single-layer and engineered multilayer appliances. During cyclic loading tests, aligners frequently exhibited cyclic hardening, marked by an initial rise in stiffness that eventually stabilised. Single-layer appliances such as Duran, Duran+, and F22 generally showed higher baseline stiffness than multilayer configurations like Erkoloc-Pro, Durasoft, CA-medium, and Zendura FLX. Furthermore, thicker aligners retained forces more effectively under cyclic strain and resisted arch-form distortion better than thinner options. Stress relaxation curves typically followed an initial rapid drop during the first several hours before plateauing, with elevated temperatures accelerating force loss.
Methodological quality assessments underscored persistent procedural gaps across the primary literature. When evaluating in vitro experiments with the QUIN tool, sixty-five studies lacked adequate blinding of operators, assessors, or analysts, while sixty omitted details regarding specimen randomisation, sequence generation, or allocation concealment. Over fifty studies failed to report personnel calibration or assessor reliability metrics, and forty-six omitted formal sample size calculations. Among cohort studies assessed via JBI criteria, common limitations involved unclear exposure validity and inadequate identification or handling of confounding factors. Potential financial conflicts of interest also emerged, as authors in two studies maintained corporate affiliations with aligner manufacturers, with one paper failing to disclose this connection.
Subject of Research: Systematic review of ageing effects on clear aligner properties
Article Title: Ageing effects on chemical, physical, mechanical, and morphological properties of clear aligners – a systematic review
Article References: Almotairy, N., Aleisa, F., & Alshammari, A. K. (2026). Ageing effects on chemical, physical, mechanical, and morphological properties of clear aligners – a systematic review. Progress in Orthodontics, 27(1), Article 40. https://doi.org/10.1186/s40510-026-00642-1
Image Credits: AI Generated
DOI: 10.1186/s40510-026-00642-1
Keywords: clear aligners, orthodontics, systematic review, material degradation, force decay, discolouration, thermoplastic polyurethane, PETG, directly printed aligners, water sorption, stress relaxation, surface morphology, intraoral ageing, simulated ageing, clinical implications, risk of bias, PRISMA 2020, PROSPERO, Progress in Orthodontics, polymer stability
Cite Scienmag News
Beatrice Stafford. (November 23, 2026). Clear Aligners Lose Significant Force Within 48 Hours. Scienmag. https://scienmag.com/clear-aligners-lose-significant-force-within-48-hours/
Beatrice Stafford. "Clear Aligners Lose Significant Force Within 48 Hours." Scienmag, 23 November 2026, https://scienmag.com/clear-aligners-lose-significant-force-within-48-hours/. Accessed 23 November 2026.
Beatrice Stafford. "Clear Aligners Lose Significant Force Within 48 Hours." Scienmag. November 23, 2026. https://scienmag.com/clear-aligners-lose-significant-force-within-48-hours/